| CSM
- Chlorosulphonated Polyethylene Rubber |
| Glass
Transition Temperature (°C) |
-25 |
| Room
Temperature Density (kg/m^3) |
1103
<> 1163 |
| Maximum
Working Temperature (°C) |
150 |
| Tensile
Strength (MPa) |
M/H |
| Resistance
To Tear |
M/H |
| Resistance
To Abrasion |
M |
| Compression
set @ -20°C (%) |
--- |
| Compression
set @ +23°C (%) |
--- |
| Compression
set @ +120°C (%) |
--- |
| Swelling
/ 70Hr / ASTM Oil No.3 @ 150°C (%) |
80 |
| Swelling
/ 70Hr / Fuel C @ Room Temperature (%) |
--- |
| Gas
Permeability |
VL |
| Ozone
Resistance |
H |
| Oxidation
Resistance |
VH |
| Rebound
(Hot) |
H |
| Rebound
(Cold) |
M/H |
| Heat Resistance
5 Hours (°C) |
200 |
| Heat Resistance
70 Hours (°C) |
140 |
| Heat Resistance
1000 Hours (°C) |
130 |
|
|
|